<BR>success, in my opinion, isn't electrolysis but the concentrated application
<BR>of heat, which breaks the corrosion and/or galvanic bonds between the steel
<BR>stud/bolt and the aluminum casting.
<BR>
<BR></FONT><FONT  COLOR="#000000" SIZE=3 FAMILY="SANSSERIF" FACE="Arial" LANG="0"></BLOCKQUOTE>
<BR></FONT><FONT  COLOR="#000000" SIZE=2 FAMILY="SANSSERIF" FACE="Arial" LANG="0">
<BR> I agree with Jeff 100%, the repeated heating and cooling effect of building 
<BR>up the bead would break the lock between the threads of the stud and the hole.